Colour fastness to rubbing: dry and wet tests

How to read separate dry and wet rubbing results, agree acceptance criteria and prepare a fabric enquiry before a production purchase.

Colour fastness to rubbing describes how much a textile’s colour transfers to another material through rubbing. For purchasing, request separate dry and wet test results with the method and conditions. An approved fabric shade alone does not establish that it will leave light-coloured lining or clothing unstained.

What is being tested

ISO 105-X12:2016 addresses colour transfer through rubbing and staining other materials. It provides for tests using a dry rubbing cloth and a wet rubbing cloth. In the wet version, the contact cloth is wetted; this does not mean arbitrarily soaking a finished bag.

This addresses a different property from mechanical surface breakdown. Martindale abrasion resistance cycles cannot replace a colour-transfer assessment. A rubbing result also does not establish fastness to washing, perspiration or light: request the corresponding tests for the exposures that matter.

How to read a grade

Check what was assessed and which scale was used in the report. ISO 105-A03:2019 describes the grey scale for assessing staining of adjacent fabrics. This transfer assessment is not a percentage of colour retained or a measure of shade matching between two components.

Keep the dry and wet results separate. If a data sheet states only “colour fastness: 4”, clarify the exposure, method, scale and exact specimen version. One number is insufficient to compare two fabrics.

A purchasing decision example

Hypothetical example: you have agreed at least grade 4 for dry and grade 4 for wet rubbing for your product, under a specified method and conditions. The supplier reports grade 4 dry and grade 3 wet. The dry requirement is met; the wet requirement is not. Averaging the results to 3.5 does not correspond to either agreed criterion.

These numbers are not a universal requirement, a DELIM test result or a product specification. Agree the requirements for your construction first, then assess the document. If the wet result is missing, record it as unverified rather than treating it as equal to the dry result.

Which specimen should represent the batch

Identify the item reference, colour or print, batch and tested fabric side. For a printed fabric, also agree the sampling area so the result concerns the required version. The DELIM catalogue includes CORDURA Westridge 500D Multicam; the brand and print name alone do not specify its dry or wet rubbing grade. Confirm that from documentation for the exact material.

When comparing reports, check the method edition, specimen preparation, dry or wet conditions, wetting parameters and assessment scale. An assembly check with the actual light-coloured lining can support selection, but it cannot replace a standard test or produce a laboratory grade.

What to include in a DELIM enquiry

  • The product, rubbing location and material that will contact the fabric.
  • Item reference, colour or print, fabric side and available sample.
  • Required dry and wet results, method and acceptance criteria.
  • Preparation, care and additional exposures relevant to the product.
  • Available reports, unverified details and approximate purchase quantity.

Browse CORDURA fabrics in the catalogue and send the manager your production requirement. For visually approving a component set, see the separate article on matching fabric and hardware colours. The version, documentation, availability and supply terms are confirmed for the specific enquiry.