Selecting elastic tape requires knowing how far it extends under a specified load and how long it is after that load is removed. Two tapes can extend equally yet recover differently. Complete a specification such as “50% stretch” with the measurement conditions and the result after the specimen has rested.
Three properties to keep separate
Elongation under load describes the increase relative to the initial gauge length. A comparison needs the force at which it was obtained, or the specified extension at which force is measured. A percentage without this condition does not describe how firmly the tape will resist stretching.
Residual extension describes the length increase remaining after unloading and an agreed recovery time. Recovery can be expressed as the fraction of the imposed extension that has disappeared. Check the definition and basis of each percentage in the report: residual extension relative to the initial length and recovery relative to the length increase use different denominators.
Example: 100, 150 and 105 mm
This is a hypothetical arithmetic example, not a DELIM test, a product specification or a standard test procedure. Let the initial gauge length L0 = 100 mm, the length under an agreed load L1 = 150 mm, and the length after unloading and the agreed rest L2 = 105 mm.
- Elongation relative to initial length: (L1 − L0) / L0 × 100 = 50%.
- Residual extension relative to initial length: (L2 − L0) / L0 × 100 = 5%.
- Fraction of the imposed extension recovered: (L1 − L2) / (L1 − L0) × 100 = 90%.
Under this convention, 5% residual extension corresponds to 90% recovery of the imposed increase. Calculating “100 − 5 = 95% recovery” would change the reference basis. For an actual report, use the definitions of the selected method.
Which conditions to agree for comparison
Record the initial gauge length and how it is established, including pretension if required. Add the force or target extension, dwell time, cycle count, recovery time and specimen preparation. Compare specimens prepared and tested under matching conditions.
ISO 20932-3:2018 addresses the elasticity of narrow fabrics; the ISO page also lists a 2025 amendment. Agree the applicable method and edition with the laboratory. ISO 20932-1 excludes narrow fabrics from its scope, so it should not automatically be applied to tape.
A single extension does not establish performance after many cycles. For example, SATRA TM103 separately describes repeated stretching and damage assessment, including after artificial ageing. This illustrates a different test question; it does not claim that a particular tape has been tested.
Moving to a specific product
The DELIM catalogue includes Pasamon TG702 elastic furniture webbing. Its furniture application does not establish suitability for every seat or transfer its properties to garment elastic. Confirm the exact version, fixing method and performance in your construction.
For the assembled sample, agree pretension, working movement, attachment and an acceptance criterion. Distinguish working elongation from elongation at break: the latter alone does not define a permissible operating range. For mechanical properties of fabric, see the separate article on tensile and tear strength.
What to send the manager
- The assembly’s purpose, a sketch and the tape fixing method.
- An item reference or sample, width, thickness, length and colour.
- Required elongation at a stated force, or force at a specified extension.
- Recovery, cycling, care and preparation conditions relevant to the product.
- Acceptance criteria, available reports and approximate quantity.
Browse elastic furniture webbing and send DELIM your production requirement. The manager will clarify the version, documentation and supply terms. This article does not set a universal stretch requirement for all products.